Reflowed two 0805 caps on two qfp protoboards. One at 250 and one at 240c.p Both took about 30 seconds to reflow. Anyone know the optimal temp for crappy old lead solder paste? Board at 250 looks scorched but that could be from the reflow oven instead. Will do a second test to find out.